PRODUCT

CHLOROSULFONATED POLYETHYLENE CSM

  • Product name: CHLOROSULFONATED POLYETHYLENE CSM
  • Product Classification: CHLOROSULFONATED POLYETHYLENE CSM
  • Company name: WEIFANG UNITE NEW MATERIALS CO.,LTD
Details
Inquiry

Chemical Properties:

1. CSM  rubber is a kind of off white, ordorless evenly rubber-shape, and it has the mutual character with rubber which also has its own property.

2. It is non-toxic, non-explosive, open flame burning, auto-extinction after removal.

3. It has excellent ozone resistance, resistance to atmospheric aging, chemical resistance, better physical mechanical, thermal aging resistance and low temperature resistance (-20℃-12℃), oil resistance, flame resistance, abrasion resistance and electrical insulation etc.

4. This rubber is a material with Neoprene Polychloroprene plus other qualities. The CSM rubber is suitable for continuous use up to about 130-degree Celsius. Chlorosulfonated polyethylene (CSM) is known for its excellent resistance to atmospheric conditions and good resistance to chemicals. Chlorosulfonated polyethylene is used in a variety of industrial and automotive applications that require high performance and have to withstand extreme weather conditions. Some products where chlorosulfonated polyethylene rubber is used include rubber linings, hoses, valve seals and gaskets etc.

Specifications:

Chloro-sulfonated polyethylene CSM4035



Property

 

   Test method

 

Unit

 

Standard

 

Chlorine content

 

GB/T 30290

 

%

 

35±2

 

Sulfur content

 

GB/T 30290

 

J/g

 

1.0-1.5

 

Volatile matter

 

GB/T 2914

 

%

 

≤0.5

 

Tensile strength

 

GB/T 528

 

Mpa

 

≥18

 

Elongation at break

 

GB/T 528

 

%

 

≥250

 

Mooney viscosity

 

GB/T 1232.1

 

ML(1+4) 100

 

40-50


Chloro-sulfonated polyethylene CSM5035





Property

 

Test method

 

Unit

 

Standard

 

Chlorine content

 

GB/T 30290

 

%

 

35±2

 

Sulfur content

 

GB/T 30290

 

J/g

 

1.0-1.5

 

Volatile matter

 

GB/T 2914

 

%

 

≤0.5

 

Tensile strength

 

GB/T 528

 

Mpa

 

 

≥20

 

Elongation at break

 

GB/T 528

 

%

 

≥250

 

Mooney viscosity

 

GB/T 1232.1

 

ML(1+4) 100

 

50-60



Chloro-sulfonated polyethylene CSM8035




Property

 

 Test method

 

Unit

 

Standard

 

Chlorine content

 

GB/T 30290

 

%

 

35±2

 

Sulfur content

 

GB/T 30290

 

J/g

 

1.0-1.5

 

Volatile matter

 

GB/T 2914

 

%

 

≤0.5

 

Tensile strength

 

GB/T 528

 

Mpa

 

≥23

 

Elongation at break

 

GB/T 528

 

%

 

≥250

 

Mooney viscosity

 

GB/T 1232.1

 

ML(1+4) 100

 

80-100


Chloro-sulfonated polyethylene CSM6035




Property

 

 Test method

 

Unit

 

Standard

 

Chlorine content

 

GB/T 30290

 

%

 

35±2

 

Sulfur content

 

GB/T 30290

 

J/g

 

1.0-1.5

 

Volatile matter

 

GB/T 2914

 

%

 

≤0.5

 

Tensile strength

 

GB/T 528

 

Mpa

 

≥22

 

Elongation at break

 

GB/T 528

 

%

 

≥250

 

Mooney viscosity

 

GB/T 1232.1

 

ML(1+4) 100

 

60-70

Application:

CSM Rubber can be used in a variety of automotive hoses, hoses, rubber compounds, special rubber rollers, seals, wire and cables, anti-corrosion coatings, waterproofing membranes, specialty tapes, rubber roller, adhesives and other special rubber products.

This rubber has excellent resistance to oxygen, ozone and most chemicals, water.

Chlorosulfonated Polyethylene Rubber has poor fuel resistance.

Hypalon CSM also has poor compression set resistance which limits its utility in dynamic sealing applications.

» It also has poor compression set resistance which limits its usefulness in dynamic sealing applications.

» It is resistant to weather.

» is also resistant to abrasion.


TEL:+86-18661828606       PHONE:+86-18661828606
E-MAIL:cpe135@vip.126.com 
ADDRESS:Binhai Economic Development Zone, Weifang, Shandong, China